The strength of Al2O3/SiC nanocomposites after grinding and annealing
HZ Wu, CW Lawrence, SG Roberts, B Derby
Acta materialia 46 (11), 3839-3848, 1998
1021998
Subsurface damage analysis by TEM and 3D FIB crack mapping in alumina and alumina/5vol.% SiC nanocomposites
HZ Wu, SG Roberts, G Möbus, BJ Inkson
Acta Materialia 51 (1), 149-163, 2003
832003
Progress in study of dispersion and stability of ceramic slurries (陶瓷料浆稳定分散进展)
R Wu), H Wu)
陶瓷学报 20 (001), 35-40, 1999
72*1999
Residual stress and subsurface damage in machined alumina and alumina/silicon carbide nanocomposite ceramics
H Wu, SG Roberts, B Derby
Acta materialia 49 (3), 507-517, 2001
702001
Engineering Structure Ceramics(工程结构陶瓷)
G Ruisong, C Su, J Huiming, W Houzheng
天津大学出版社 (Tianjin University Press), 2002
51*2002
A high entropy silicide by reactive spark plasma sintering
Y Qin, JX Liu, F Li, X Wei, H Wu, GJ Zhang
Journal of Advanced Ceramics 8 (1), 148-152, 2019
462019
Residual stress distributions around indentations and scratches in polycrystalline Al2O3 and Al2O3/SiC nanocomposites measured using fluorescence probes
HZ Wu, SG Roberts, B Derby
Acta materialia 56 (1), 140-149, 2008
422008
Friction surface evolution of carbon fibre reinforced carbon/silicon carbide (Cf/C-SiC) composites
Y Wang, H Wu
Journal of the European Ceramic Society 30 (15), 3187-3201, 2010
332010
Local ordering of oxygen vacancies in cubic zirconia (ZrO2) stabilized with yttria (Y2O2) and magnesia (MgO) I. Electron diffuse scattering study
ZR Dai, ZL Wang, YR Chen, HZ Wu, WX Liu
Philosophical Magazine A 73 (2), 415-430, 1996
321996
Microstructure of friction surface developed on carbon fibre reinforced carbon–silicon carbide (C f/C–SiC)
Y Wang, H Wu
Journal of the European Ceramic Society 32 (12), 3509-3519, 2012
292012
冷冻干燥法制备 MgO—ZrO2 超细粉末 (Preparation of ultra-fine MgO-ZrO2 powder by frozen-drying
J Liu), H Wu)
硅酸盐学报 (Journal of the Chinese Ceramic Society) 24 (001), 105-108, 1996
26*1996
Contact damage of silicon carbide ceramics with different grain structures measured by Hertzian and Vickers indentation
J Wade, S Ghosh, P Claydon, H Wu
Journal of the European Ceramic Society 35 (6), 1725-1736, 2015
232015
Josephson fluxon flow and phase diffusion in thin-film intrinsic Josephson junctions
PA Warburton, AR Kuzhakhmetov, OS Chana, G Burnell, MG Blamire, ...
Journal of applied physics 95, 4941, 2004
202004
Fracture toughness of a zirconia engineering ceramic and the effects thereon of surface processing with fibre laser radiation
PP Shukla, J Lawrence, H Wu
Proceedings of the Institution of Mechanical Engineers, Part B: Journal of …, 2010
192010
Mechanical behaviour of the constituents inside carbon-fibre/carbon-silicon carbide composites characterised by nano-indentation
A Leatherbarrow, H Wu
Journal of the European Ceramic Society, 2011
182011
Buffer layers for Tl-2212 thin films on MgO and sapphire substrates
SC Speller, H Wu, CRM Grovenor
IEEE transactions on applied superconductivity 13 (2), 2713-2716, 2003
182003
Synergetic roles of ZrC and SiC in ternary ZrB 2–SiC–ZrC ceramics
HL Liu, GJ Zhang, JX Liu, H Wu
Journal of the European Ceramic Society 35 (16), 4389-4397, 2015
172015
Friction performance of carbon/silicon carbide ceramic composite brakes in ambient air and water spray environment
G Bian, H Wu
Tribology International 92, 1-11, 2015
172015
Plasma augmented laser welding of 6 mm steel plate
PT Swanson, CJ Page, E Read, HZ Wu
Science and Technology of Welding &# 38; Joining 12 (2), 153-160, 2007
172007
3D mapping of subsurface cracks in alumina using FIB
BJ Inkson, HZ Wu, T Steer, G Möbus
MRS Online Proceedings Library Archive 649, 2000
162000